Recently, I have been busy analyzing and solving the problems of non-conforming and unstable shell dimensions. Previously, I also posted an article on GD&T (Geometric Dimensioning and Tolerancing).

In this article, I will share some common problems in shell machining and my approaches to analyzing and solving them.

New energy electric drive shells are probably the highest precision die-casting parts in terms of dimensional accuracy. The bearing hole of the electric drive shell is a critical part of the drive system. Its machining quality directly affects bearing assembly accuracy, transmission efficiency, and equipment life.

The machining accuracy of motor parts is one of the important factors affecting motor performance and life. Controlling machining accuracy in motor part manufacturing is crucial for enhancing motor performance, reducing noise, extending service life, and improving product quality.

 

Common defects in die-casting shells, their causes and solutions are as follows:

 I. Dimensional Accuracy Issues

1. Main problems: Over tolerance in hole diameter (too large or too small), insufficient roundness and cylindricity, over tolerance in positional tolerance, coaxiality deviation of multiple holes, and insufficient perpendicularity between hole axis and end face.

2. Possible causes: Tool wear or improper parameters (e.g., feed rate, speed); insufficient rigidity of tools or fixtures causing machining vibration; thermal deformation due to temperature changes; unreasonable sequencing, inconsistent machining datum (e.g., multiple clamping errors); machine tool geometric accuracy issues (e.g., spindle runout).

3. Conventional solutions:

Tool optimization: Use coated carbide tools or CBN tools. Monitor tool life automatically and check tool wear regularly.

Process parameter optimization: Select reasonable cutting parameters to ensure cutting quality and dimensional accuracy. Divide the process into rough machining (leaving allowance) and finish machining (low-speed, high-precision cutting).

Process optimization: Optimize machining sequence, reduce process steps, and minimize errors from multiple clamping and positioning.

Temperature control: Maintain a constant temperature in the machining environment and for cutting fluid.

High-precision equipment: Use high-precision four-axis/five-axis machining centers to ensure stable accuracy. Select appropriate tooling and fixtures to improve positioning and clamping accuracy.

Inspection and compensation: After machining, inspect with a CMM (Coordinate Measuring Machine). If necessary, revise the machining path and choose the optimal evaluation and calculation logic for positional tolerance.

 II. Surface Appearance Quality Issues

1. Problem manifestations: Surface roughness not up to standard (Ra>1.6μm), scratches, vibration marks, burrs, gas pores, sand holes.

2. Possible causes:

- Improper cutting parameters (e.g., excessive feed rate)

- Chipped tool edges or poor chip evacuation

- Inhomogeneous material hardness (e.g., hard spots in castings)

- Improper casting process control

3. Common solutions:

- Parameter optimization: Reduce feed rate and increase spindle speed for small-depth finishing.

- Deburring: Use forming tools or special tools to remove burrs from hole openings.

- Tool optimization: Select suitable tools for chip breaking to prevent chip winding.

 III. Preventive Measures

1. Process monitoring: Use an online measurement system for real-time feedback and compensation of machining dimensions.

2. Maintenance plan: Regularly calibrate machine tool spindle accuracy.

3. Include spindle and tool holder aluminum chip issues in daily inspections.

4. Install tool breakage detection and tool life monitoring systems for automatic alerts.

5. Equip tooling with air gap detection systems to prevent clamping abnormalities.

 IV. Common Machining Processes and Tools for Bearing Holes

There are two common materials for motor shell bearing holes. One is a steel sleeve (commonly made of 45# steel, 40Cr, or stainless iron) inserted into a die-casting shell. The other is a hole made of the die-casting shell's own aluminum material.

Common machining tools include reamers and boring tools. Adjustable reamers are widely used due to their time-saving advantages in reducing tool removal, measurement, and waiting times, thereby improving production efficiency and stability.

 

For most electric drive shell bearing holes with tolerances within 2 wire, using non-adjustable reamers can easily lead to undersized products due to slight tool wear. Die-casting aluminum shell bearing holes are relatively easier to machine with better dimensional stability. However, the most problematic bearing holes are the inserted sleeves. Machining steel materials can easily result in tool wear, chipping, and wire wrapping, causing bearing holes. If not detected in time, this may lead to batch defects. Therefore, selecting appropriate tools and processes is crucial.

 

With the innovation of tool developers, there are now good reamers for machining steel sleeves on the market. We have verified and compared them in actual production. The following figure shows a high-speed, high-line-speed dedicated reamer. For D80 steel sleeve bearing hole precision reaming, the cycle is 1-3 seconds per hole, and it can stably machine φ62-120mm steel sleeve bearing holes for 2000-5000 cycles. Adjustment is simple, requiring only a torque of≈25N/m and an Allen key for easy adjustment. Each click compensates precisely 0.005mm. The tool can be adjusted directly on the machine without removal. This also solves chip breaking problems, eliminating worries of iron chips damaging part surfaces. The tool life maintains a surface roughness of Ra1.6 or below, ensuring processing life, improving efficiency, and guaranteeing product quality. According to tool manufacturers, this adjustable reamer can machine hole diameters ranging from 12-120mm.

 

Additionally, clients often require limit samples. With this tool, there is no need to make new or remove tools for adjustment. Direct machine adjustment can quickly meet the requirements for limit sample production. Compared to single-edged adjustable boring tools, multi-edged reamers offer better dimensional stability, efficiency, and internal surface roughness. However, single-edged tools may be less suitable for smaller holes and may provide slightly inferior cylindricity and roundness stability.

 

In my experience, single-edged tools pose greater challenges in tool life and dimensional stability when machining steel sleeve holes. For steel sleeve holes with oil grooves or notches requiring intermittent cutting, higher demands are placed on tool structure and insert selection. The tool must ensure longevity, dimensional stability, and machining efficiency, making adjustable reamers a better choice.

Of course, machining dimensional stability is not solely reliant on tools. Other factors such as fixture stability, rough machining allowance, and machine spindle rigidity must also be controlled. The processing of root slots at the bottom of steel sleeve holes is particularly important. Regardless of the tool type, all factors affecting dimensional stability must be comprehensively monitored.

 

In actual mass production of die-casting shells, batch defects often occur due to tool life expiration or insufficient dimensional inspection after tool replacement. Therefore, in production, the 5M1E factors must be well monitored, and single-piece product traceability must be ensured.

 

The machining accuracy of motor components is one of the key factors in ensuring motor performance and life. To guarantee this accuracy, a comprehensive approach considering material selection, machining processes, equipment and tools, and process control is necessary. A robust quality control system with strict inspections should be established to ensure compliance with accuracy requirements. Process improvements and modern inspection methods can further enhance machining accuracy and stability.
 

Send Inquiry