Fusion welding (referred to as fusion welding) is a process that uses thermal energy (such as electrical energy, chemical energy, etc.) to locally heat and melt two separate metal workpieces, and tightly and securely connect them into a whole through the combination and diffusion of atoms or molecules.
Fusion welding is essentially similar to steel smelting, achieving its process through melting and crystallization stages. However, from a technical standpoint, they are quite different. The characteristics of welding processes are as follows:
1. The heat source is mobile
During welding, the heat source (such as an electric arc, gas flame, etc.) moves along the joint in a certain direction from one end to the other in a regular pattern. Due to the instability of the moving heat source and the variability of welding parameters, the control of the temperature in the molten pool and the assurance of weld quality are more difficult.
2. The heat source is high in temperature and concentrated
The heat source is compressed into a very small volume due to its own (such as the diameter of the welding rod) or external factors, and the corresponding temperature is also very high. For example, the flame temperature of gas welding is about 3000K; the arc column temperature of electric welding is about 5000-8000K; the arc column temperature of tungsten inert gas welding is as high as over 10000K.
3. The volume of heated metal is small
During welding, the heat source only acts on a local part of the overall metal workpiece, and the heated area is very small. The size of the molten pool is determined by the cross-sectional area of the welding material and the heat source, generally only 2-10 cubic centimeters.
4. The melting and solidification time is short
During welding, the time for each weld point's metal to melt and then cool and solidify is very short, usually measured in minutes or seconds.
5. High temperature gradient
Under the action of the heat source, a point on the welded metal melts, and the further away from the heat source, the lower the temperature of the metal. This temperature difference is called the temperature gradient. The size of the temperature gradient is related to the thickness of the welded workpiece, the welding line energy, and the thermal conductivity of the metal. The thicker the weld piece, the larger the line energy, and the worse the thermal conductivity, the greater the temperature gradient formed.
6. Unbalanced chemical reactions
During the welding process, due to the short melting and solidification time of the molten metal, the chemical reactions between metal, gas, and slag have not fully proceeded before solidification. The gas and slag in the weld do not have time to escape and remain in the weld as defects such as pores and slag inclusions. At the same time, some chemical elements are also fixed before they can be evenly distributed, leading to segregation.
7. Changes in chemical composition and microstructure
The pool of molten metal and the droplets of welding material come into contact with the surrounding air, and the evaporation and decomposition of oil, rust, and paint on the metal surface, as well as humid environments, can leave harmful gases such as oxygen, nitrogen, and hydrogen in the weld, forming various defects. At the same time, the chemical composition of the metal is severely burned or undergoes migration and diffusion under high temperatures, causing unevenness in chemical composition.
Under the action of the heat source, the microstructure of the metal also changes. For example, a typical and coarse casting structure is an example. Since the solidification speed of the metal is very fast, welds with a high tendency to harden can easily form martensitic quenched structures.
8. Changes in the microstructure of the base metal
The base metal near the molten pool, which is not melted, will undergo a change in its structure due to heat, and this part is called the heat-affected zone. For carbon steel, this zone inevitably contains overheated structures (such as Widmanstätten structure). For alloy steel, it is easy to form hardening structures.
It can be seen that although fusion welding has certain advantages, due to the above-mentioned technical characteristics, it brings a series of difficulties to the welding process. Therefore, it is necessary to update and improve from the aspects of equipment, welding materials, and process technology to obtain excellent welds.
Conclusion
Fusion welding is a critical process in various industries, utilizing thermal energy to melt and join metals. It's characterized by a mobile heat source, high temperatures, small heated volumes, and short melting times, which lead to challenges in quality control. Despite these, fusion welding is widely used in aerospace, automotive, power, shipbuilding, construction, and heavy industries for its strength and versatility. It's also essential for joining dissimilar metals and in electronics and military manufacturing. As technology advances, fusion welding becomes more efficient and environmentally friendly, expanding its applications in modern production.