What are the characteristics and application ranges of brazing in welding?

Dec 26, 2024

Leave a message

In the rapidly developing modern industry, metal has become an indispensable material. To turn these metal materials into industrial products, connection is inevitable, and welding is one of the main processing methods to connect these components. Brazing technology holds irreplaceable importance in welding. As a basic process and technology in manufacturing, brazing has made significant contributions to industrial economic development. In fields that humans take pride in, such as aerospace, nuclear energy utilization, and electronic information, the advanced achievements of brazing technology have been utilized. As China is on its way to becoming the "world's factory," with the needs of economic development, it is believed that brazing technology will develop more rapidly and play a more important role in industrial production.

 

Meaning and Characteristics of Brazing Technology:

Brazing is a process that uses a filler metal (brazing material) with a lower melting point than the base material. The base materials are heated together without melting, causing the filler metal to melt, wet, and fill the gap at the connection point of the base materials, forming a weld. In the brazed joint, the filler metal and the base material dissolve and diffuse into each other, forming a solid bond. In the past, brazing was also called soldering or low-temperature welding, and it has different points compared to fusion welding. First, the base material does not melt during brazing, only the filler metal melts. Second, in the brazed joint, the composition and properties of the filler metal are significantly different from the base material. Additionally, brazing relies on the molten filler metal filling the joint gap under capillary action, which does not occur in fusion welding.

Compared to fusion welding, brazing has a lower heating temperature, resulting in minimal changes to the organization and mechanical properties of the weldment, less deformation, smooth and aesthetically pleasing joints, and the ability to connect different materials. However, brazing also has obvious shortcomings, such as lower joint strength, which is why lap joints are often used to provide load-bearing capacity. At the same time, brazing requires higher assembly precision than fusion welding, ensuring strict gaps and cleanliness of the base materials. Welding methods are usually named after the heat source and heating method, such as flame brazing, soldering iron brazing, resistance brazing, induction brazing, and furnace brazing.
 

Brazing Process:

1. The steps included in the brazing process are:
- Workpiece surface treatment, including degreasing, removing excess oxide scale, and sometimes plating the workpiece that will be brazed.
- Assembly and fixation to ensure the relative position of parts remains unchanged.
- Optimal placement of filler metal and flux to ensure liquid filler metal can flow through complex joints in the most streamline direction.
- When filler metal flows over the workpiece surface and does not enter the joint, a blocker may be applied to regulate the flow of filler metal.
- Correct selection of brazing process parameters, including brazing temperature, heating rate, holding time after joint completion, and cooling rate.
- Post-brazing cleaning to remove flux residues that may cause corrosion or deposits that affect appearance.
- If necessary, the brazed joint and the entire workpiece should also be post-brazed plated, for example, with other inert metal protective layers, passivation treatment, painting, etc.

2. Key points of brazing operation:
- Flame brazing operations usually involve manually adding wire filler metal or preplacing filler metal on the joint. Flux is applied to the brazing parts before heating to protect the base material from oxidation during the heating process. To prevent the flux from being blown away by the flame, it can be mixed with water or alcohol to form a paste. During brazing operations, the flame should slowly heat the entire joint area to allow the moisture in the flux to evaporate first. Additionally, the heated end of the wire filler metal can be periodically dipped into the flux to pick up the flux and then bring it to the heated base material. To uniformly heat the base material, the distance between the torch and the heating area of the base material should be controlled at about 70-80mm. It is particularly important to note that flame brazing operations are different from gas welding operations. Gas welding often starts heating from one end of the weld, concentrating the flame on one point to form a molten pool, and then continuously heats forward; whereas flame brazing first heats the entire joint area with the outer flame to reach the brazing temperature, and then continues to heat from one end with the flame, allowing the braze to quickly flow into the continuously heated joint gap.
 

Types of Brazed Joints and Operational Points:

1. Types of brazed joints: Brazed joints are usually dominated by butt and lap joints.
- Butt joints: The combination strength is lower than the base material and mainly fails along the braze when loaded, so it is only suitable for brazing of unimportant and low-load parts.
- Lap joints: To fully utilize all the advantages of brazing, brazed joints often use lap joints. By changing the degree of overlap (the fillet is more than three times the plate thickness, but generally not more than 15mm), the brazed joint can achieve equal strength with the base material. Therefore, when designing brazed joints, do not simply copy the type of fusion welding joints. Special attention should be paid to the following when designing brazed joints:
- The braze seam in the joint should be as parallel to the direction of force as possible.
- To ensure uniform heating and stress distribution, the thickness in the joint area should be as close as possible.
- Do not form corners in the joint that hinder the clear action of the filler metal.

2. Assembly clearance of brazed joints: When assembling brazed joints, correctly choosing the gap size is an important factor in determining the density of the braze seam. If the gap is too small, due to uneven contact surfaces, it will hinder the flow of the filler metal. Conversely, if the gap is too large, it will destroy the capillary action of the gap, and the filler metal will not fill the gap of the joint.

The size of the gap is directly related to the properties of the filler metal and base material, brazing temperature, brazing time, and placement of the filler metal. Generally, if the interaction
between the filler metal and the base material is weak, a smaller gap is required. It should be noted that the gap required here refers to the gap at the brazing temperature, which may not be the same as at room temperature.
 

Types of Braze Seams and Flowability of Filler Metal in Braze Seams:

There are various types of braze seams, and manuals and books on brazing generally have detailed designs and drawings. Summarized, for butt and lap joints of plates and tubes, there are only three types of braze seams: face-to-face (e.g., butt joints), surface-to-surface (e.g., lap joints), and face-to-surface (e.g., "T" joints). In fact, specific braze seams are often not single. Molten filler metal flows in a straight line in the braze seam, and the capillary action of the braze seam plays a significant role, which is related to the type of braze seam and the size of the braze seam gap. Generally, a smaller braze seam gap has better straight-line flowability than a larger gap. However, it is not the smaller the better. The optimal value of the braze seam gap is between 0.01-0.2mm, and the specific value depends on the type of base material. A larger braze seam section (larger lap area) will have greater load-bearing capacity. To improve the joint strength of the braze seam, when making butt joints, the joint is usually processed into a 30° beveled end to increase the connection cross-section of the butt braze seam and provide load-bearing capacity; when making lap joints, the general lap length is about three times the plate thickness, generally not more than 15mm.
 

Application of Brazing Technology in Reality

Brazing is primarily used in the manufacturing of precision instruments, electrical components, dissimilar metal structures, and complex thin-walled structures. During brazing, the contact surfaces of the workpieces to be brazed are cleaned, assembled in a lap joint configuration, and the filler metal is placed near or directly into the joint gap. When the workpieces and filler metal are heated together to a temperature slightly above the melting point of the filler metal, the filler metal will melt and wet the surfaces of the workpieces. The liquid filler metal, aided by capillary action, flows and spreads along the seam. This allows for mutual dissolution and penetration between the brazed metal and the filler metal, forming an alloy layer that, upon condensation, creates a brazed joint. Brazing is generally divided into soft soldering and hard soldering based on the melting points of the filler metals: soft soldering uses filler metals with melting points below 450°C and results in joints with lower strength (less than 70MPa). Soft soldered joints have lower strength and are suitable for welding components that small loads or operate at lower temperatures but require good sealing. They are commonly used in the electronics and food industries for welding electrically conductive, gas-tight, and water-tight devices. Tin soldering, which uses tin-lead alloy as the filler metal, is the most commonly used. There are many types of flux, and in the electronics industry, rosin-alcohol solutions are often used for soft soldering. This type of flux leaves no corrosive residue on the workpieces after welding, known as non-corrosive flux; hard soldering uses filler metals with melting points above 450°C, resulting in joints with higher strength (greater than 200MPa). It can be used to connect parts that heavy loads or operate at high temperatures. Examples include: hard alloy tools, drilling bits, bicycle frames, heat exchangers, conduits, and various containers; in the manufacturing of microwave waveguides, electron tubes, and electronic vacuum devices, brazing is often the only possible joining method. Hard soldering filler metals are diverse, with those based on aluminum, silver, copper, manganese, and nickel being the most widely used. Aluminum-based filler metals are commonly used for brazing aluminum products. Silver-based and copper-based filler metals are often used for brazing copper and iron parts. Manganese-based and nickel-based filler metals are mostly used for brazing stainless steel, heat-resistant steel, and high-temperature alloy parts that operate at high temperatures.
 

Concluding Remarks

In recent years, due to the development of new technologies in aviation, aerospace, nuclear energy, and electronics, as well as the adoption of new materials and new structural forms, higher demands have been placed on connection technologies. As a result, brazing technology has gained greater attention and has rapidly developed, leading to the emergence of many new brazing methods. For instance, various drilling and mining tools processed using new brazing methods can now meet the requirements for deep or ultra-deep drilling: components such as water tanks for power machinery, motor components, and blades and tension members of steam turbines have begun to adopt brazing technology. Even in nuclear power plants and naval nuclear propulsion devices, important components such as fuel element positioning frames, heat exchangers, and neutron detectors have widely adopted brazing technology. In short, brazing technology will continue to develop with the advancement of science and technology, and expand into broader fields and deeper levels.

Send Inquiry